11.12.2012 Views

continued from part 1 - Controller General of Patents, Designs, and ...

continued from part 1 - Controller General of Patents, Designs, and ...

continued from part 1 - Controller General of Patents, Designs, and ...

SHOW MORE
SHOW LESS

You also want an ePaper? Increase the reach of your titles

YUMPU automatically turns print PDFs into web optimized ePapers that Google loves.

(12) PATENT APPLICATION PUBLICATION (21) Application No.6632/DELNP/2008 A<br />

(19) INDIA<br />

(22) Date <strong>of</strong> filing <strong>of</strong> Application :30/07/2008 (43) Publication Date : 24/10/2008<br />

(54) Title <strong>of</strong> the invention : LIGHTWEIGHT THIN FLEXIBLE POLYMER COATED GLOVE AND A METHOD THEREFOR<br />

(51) International classification :C04B 35/01 (71)Name <strong>of</strong> Applicant :<br />

(31) Priority Document No :PCT/ES2005/070191 1)FAJARDO SOLA, PEDRO<br />

(32) Priority Date :30/12/2005<br />

Address <strong>of</strong> Applicant :C/MARQUES DEL TURIA 1, E-46930<br />

(33) Name <strong>of</strong> priority country :PCT<br />

QUART DE POBLET SPAIN Spain<br />

(86) International Application No :PCT/ES2005/070191 (72)Name <strong>of</strong> Inventor :<br />

Filing Date<br />

:30/12/2005<br />

1)FAJARDO SOLA, PEDRO<br />

(87) International Publication No :WO 2007/077267<br />

(61) Patent <strong>of</strong> Addition to Application<br />

Number<br />

Filing Date<br />

:NA<br />

:NA<br />

(62) Divisional to Application Number :NA<br />

Filing Date<br />

:NA<br />

(57) Abstract :<br />

The invention relates to an improved refractory coating for ladles used in the stainless steel industry in order to prevent any interaction<br />

between brick <strong>and</strong> slag, which has a determinant effect on the deteroriation <strong>of</strong> the coating in the absence <strong>of</strong> aforementioned reaction,<br />

the other destructive effects <strong>of</strong> the bricks have a reduced affect. The exact purpose <strong>of</strong> the invention is to prevent the brick/slag<br />

interaction using a brick that is compacted under high pressure with a density <strong>of</strong> more than 3 kg/decimetre3 <strong>and</strong> a porosity <strong>of</strong> less than<br />

4%. The said brick has a composition containing between 66-68 wt % Magnesite (MgCO3), between 14-15 wt% Alumina (A1203),<br />

<strong>and</strong> between 9-10 wt% Graphite, as well, between 7-9 wt% <strong>of</strong> additives that are used to improve thermal shock, heat resistance <strong>and</strong><br />

oxidation in a combined composition <strong>of</strong> Aluminium powder, Silicon metal, Silicon carbide, <strong>and</strong> clay). Moreover, the invention<br />

comprises between 2-3 wt% phenolic resins by weight <strong>of</strong> a binder, in relation to the total percentages referred to above.<br />

No. <strong>of</strong> Pages : 9 No. <strong>of</strong> Claims : 1<br />

The Patent Office Journal 24/10/2008 26065

Hooray! Your file is uploaded and ready to be published.

Saved successfully!

Ooh no, something went wrong!