11.12.2012 Views

continued from part 1 - Controller General of Patents, Designs, and ...

continued from part 1 - Controller General of Patents, Designs, and ...

continued from part 1 - Controller General of Patents, Designs, and ...

SHOW MORE
SHOW LESS

Create successful ePaper yourself

Turn your PDF publications into a flip-book with our unique Google optimized e-Paper software.

(12) PATENT APPLICATION PUBLICATION (21) Application No.6591/DELNP/2008 A<br />

(19) INDIA<br />

(22) Date <strong>of</strong> filing <strong>of</strong> Application :29/07/2008 (43) Publication Date : 24/10/2008<br />

(54) Title <strong>of</strong> the invention : "METHOD FOR PRODUCING AN OIL-BINDING AGENT PRODUCED ACCORDING TO SAID<br />

METHOD<br />

(51) International classification :B01J 20/30 (71)Name <strong>of</strong> Applicant :<br />

(31) Priority Document No :A 110/2006<br />

1)COMMERZIALBANK MATTERSBURG IM<br />

(32) Priority Date :25/01/2006 BURGENLAND AKTIENGESELLSCHAFT<br />

(33) Name <strong>of</strong> priority country :Austria<br />

Address <strong>of</strong> Applicant :JUDENGASSE 11, A-7210<br />

(86) International Application No :PCT/AT2007/000024 MATTERSBURG,AUSTRIA. Austria<br />

Filing Date<br />

:22/01/2007 (72)Name <strong>of</strong> Inventor :<br />

(87) International Publication No :WO 2007/085031 1)PHILIPP,FRANZ JOSEF<br />

(61) Patent <strong>of</strong> Addition to Application<br />

Number<br />

Filing Date<br />

:NA<br />

:NA<br />

(62) Divisional to Application Number :NA<br />

Filing Date<br />

:NA<br />

(57) Abstract :<br />

The invention relates to a method for producing an oil-binding agent <strong>of</strong> granular open-porous structure with a silicate ceramic matrix<br />

by using recovered paper material <strong>and</strong> clay. The method is characterized in that, in each case based on the entire raw material, 35 to 60<br />

wt.-% sewage sludge with a water content <strong>of</strong> between 70 <strong>and</strong> 85 wt.-%, 25 to 55 wt.-% recovered paper material with a water content<br />

<strong>of</strong> between 35 <strong>and</strong> 55 wt.-%, 10 to 25 wt.-% clay <strong>and</strong> optionally 1 to 3 wt.-% zeolithe, 1 to 2 wt.-% quicklime <strong>and</strong>/or up to 3 wt.-% fly<br />

ash are mixed to a homogeneous mixture. The raw material thus obtained is subsequently processed in order to form <strong>part</strong>icles having<br />

an average diameter <strong>of</strong> 4 to 6 mm. The <strong>part</strong>icles are then dried <strong>and</strong> subsequently burnt at 950 to 1050 °C. The oil-binding agents<br />

produced according to said method have a bulk density <strong>of</strong> between 0.4 <strong>and</strong> 0.75 kg/1 <strong>and</strong> a oil-binding capability <strong>of</strong> 0.7 to 1.0 1 oil per<br />

oil-binder.<br />

No. <strong>of</strong> Pages : 17 No. <strong>of</strong> Claims : 12<br />