Understanding API ICP653 Reading 15-Worksheet-11a
Create successful ePaper yourself
Turn your PDF publications into a flip-book with our unique Google optimized e-Paper software.
Q3. In reviewing the form QW-483 (PQR form) in a Code shop, the<br />
Authorized Inspector noticed the thickness of test coupon was<br />
documented as 3/4" SA-285C plate. However on the back of the form<br />
thickness of the specimen was recorded as 0.725". The difference in<br />
thickness is most likely because.<br />
(a) A mistake in the testing laboratory, they documented a different set of<br />
coupon on this PQR.<br />
(b) The thickness of the specimen is approximate.<br />
(c) The test coupon has been machined down to 0.725" to offset the heat<br />
distortion due to welding.<br />
ANS: c<br />
Q4. A welder was qualified by a plate at 4G (overhead) position in the lab. He<br />
will be qualified to weld pipe 2 7/8" O.D. and over, but under 24" O.D. in<br />
the field in the overhead position.<br />
(a) True<br />
(b) False<br />
ANS: b correct answer<br />
Charlie Chong/ Fion Zhang