Design and functionSelect welding task5.10.2.5 <strong>Welding</strong> parameter ignition time "tZn" diagramNOTEIn the ignition time, the wire feed continues to run at creep speed after the arc is ignited;the ignition behaviour is improved with the optimum setting.The process described below is always used if there is a pause between welding processes ofnot less than 1.5 seconds.Figure 5-11Legend with an explanation of symbols can be found in the MIG/MAG function sequences /operating modes chapter.44099-005224-EW50108.11.2011