1. Weld at least 2 shear studs at start of each work period to determine proper generator, control unit, and<br />

stud welder settings. Bend studs 45 degrees from vertical by striking with hammer. Inspect weld. Do not<br />

include these 2 studs in required total number of studs on Project.<br />

2. Visually inspect welds at shear studs. Test studs which do not appear to have full sound 360 degree fillet<br />

weld at base. Test by bending 15 degrees from vertical toward nearest end of beam by striking with<br />

hammer. Replace studs which fail this test.<br />

3. When temperature is below 32 degrees F, test one stud in each 100 studs after weld cools. If stud fails in<br />

weld, test 2 additional studs. Do not resume welding unless 2 additional studs pass test.<br />

3.05. ADJUSTING<br />

A. Field Touch Up of Deck: After erection, use cold galvanizing compound to touch up both sides of deck at<br />

welds, weld scars, bruises, and rust spots.<br />