Retrofitting of damaged sandwich panels - EPAQ
Retrofitting of damaged sandwich panels - EPAQ
Retrofitting of damaged sandwich panels - EPAQ
Create successful ePaper yourself
Turn your PDF publications into a flip-book with our unique Google optimized e-Paper software.
Returning <strong>of</strong> resistance <strong>of</strong> <strong>panels</strong><br />
exposed to blisters or accidential attacts<br />
Artificial defects<br />
- simulation <strong>of</strong> real defects and faults<br />
Photo;<br />
Eric Rustemeijer<br />
Development <strong>of</strong> repairing actions<br />
- four different technigues<br />
- suitability to conditions on site<br />
B / 1<br />
R<br />
Experimental verification<br />
one circular dent<br />
- diameter D1 = 200 mm<br />
- depth d1= 10 mm<br />
D1<br />
EASIE MC, Roma<br />
September 21, 2011<br />
3