These raw materials are mixed according to a specific recipe to obtain a 2,000-pound charge. The materials are then transferred<br />
into a 600°F pre-heater, which removes any oil or water.<br />
melting<br />
This is an electric induction furnace. It has a four-ton capacity. The raw materials are transferred to the furnace,<br />
then melted at 2,800°F. It takes 15 minutes to melt the 2,000-pound charge into molten metal.